DEFECT TROUBLESHOOTING

تحلیل عیوب تزریق

Use defect location, wall thickness, gate, venting and trial conditions for the first diagnosis.

Real plastic part porosity defect photo from Wikimedia Commons for defect troubleshooting
Real image source: Wikimedia Commons, “Porosities in a plastic part - garden chair”, by Thibdx, licensed CC BY 4.0. Used as a real defect reference image; it is not a customer product of this company.

تحلیل عیوب تزریق

Use defect location, wall thickness, gate, venting and trial conditions for the first diagnosis.

Practical checks

Sink marks usually appear behind thick sections, bosses and ribs. Flash is often related to shutoff and mold locking. Weld lines and trapped air appear near flow meeting or last-fill areas.

Engineering review

Sudden wall changes, thick ribs, small gates or poor venting are structural and mold issues. Tuning alone rarely removes the root cause.

Discussion

Photos, material direction, wall thickness, gate location, defect position, trial parameters and quantity target make discussion more useful.

References: Protolabs Xometry Plastics Technology MoldMaking Technology
Content is rewritten and summarized from public sources; images are site-owned process illustrations.
DISCUSSION

گفت‌وگو و پرسش

می‌توانید درباره انتخاب مواد، عیوب قالب‌گیری، ساختار قالب، نمونه‌سازی یا بررسی پروژه پرسش بگذارید.

هنوز گفت‌وگویی ثبت نشده است. شما می‌توانید اولین پرسش را بگذارید.

ثبت دیدگاه

دیدگاه‌ها ممکن است پیش از نمایش بررسی شوند.